In case you are still interested in black wax, the following is supposed to be a good substitute for TCE. I undestand TCE (and TCA) are not considered evironmentally friendly these days. The commercial name is "HyperSolve". I understand it is n-propyl bromide (1-bromopropane) with some secret additive. Here's one contact for it. Grant Moskowitz Aviation and Defense Team Leader Phone: 619-269-8930 Fax: 619-269-8932 4843 Voltaire Street, Suite A San Diego, CA 92107 email: gmoskowitz@ecolink.com Visit our new web site: www.ecolink.com PS: I'm going to look into the Enthone OMI "stop-off Number 1". -----Original Message----- From: Karl Cazzini [SMTP:karlcazzini@rcn.com] Sent: Tuesday, February 26, 2002 10:38 AM To: mems-talk@memsnet.org Subject: Re: [mems-talk] black wax A much better masking material Enthone OMI "stop-off Number 1". This material is a green paint on polymeric compound which dries quickly and is completley resistant to acids and bases. It is EASILY removed, and simply peels off like a rubber sheet - no residuals. I have used the Apiezon "Black Wax" material, but not with the same degree of satisfaction (especially upon removal - it leaves residuals). K. Cazzini (Ph.D) Senior Scientist Alcon Research Ltd. > > From: "ABHIJAT GOYAL"> Date: 2002/02/25 Mon PM 10:12:59 EST > To: mems-talk@memsnet.org > Subject: [mems-talk] black wax > > Hi, > > can you please suggest me some vendors for Black Wax as a mask for KOH etch. > Can you please tell me the vendors that are based in US only, since it will be > difficult for me to procure my order if they are outside the US. > > Also can you please suggest me something by which I can remove black wax after I have etched. > > Thanks in advance, > > Abhijat Goyal > > > Abhijat Goyal > EE MEMS group, > MS candidate, > Dept. Of Electrical Engineering, > State College, PA > > Ph: (R)814-2350917 > (O)814-8653664 > _______________________________________________ > mems-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.mems-exchange.org/ _______________________________________________ mems-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.mems-exchange.org/