Try Goodfellow (www.goodfellow.com). I got PMMA sheets of varying thickness from them (500, 125 and 50 um thick.) The sheets are rather larger and you have to cut the plastic to wafer size, but it has worked well for me. They probably have different plastics as well... Jeff --- "Zhu, Xiaoshan"wrote: > Hi, there, > > Do you know which company sell some thin plastic > wafers(thickness<200um)? > > Thank you so much! > > ZHU, Xiaoshan > _______________________________________________ > mems-talk@memsnet.org mailing list: to unsubscribe > or change your list > options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS > processing services. > Visit us at http://www.mems-exchange.org/ Try FREE Yahoo! Mail - the world's greatest free email! http://mail.yahoo.com/