I have a problem spinning SU-8 2050 photoresist (Microchem corp). When I place the required amount on my 2" silicon wafer and spin, it does not spread uniformly. Instead it all goes to one side (if it is not exactly centered) or it spreads out in a starfish pattern, leaving large portions of the wafer uncovered. I have tried manually spreading the SU-8 across the wafer, with my pipette, but this introduces bubbles. It was also suggested to tilt the wafer to get the SU-8 to spread, or to sit it on a table. Neither of these suggestions worked, since the SU-8 2050 is so viscous and it takes so long to spread with gravity, a skin forms on the SU-8 before it spreads. Does anyone have suggestions? Glen Landry