Hi Amanda, we have coated the side walls of an SU-8 channel structure with a couple of different metal, platinum and copper included. We used a shadow mask type process with a stainless steel stencil as the mask. There were some problems with the metal spreading into the channel, which we resolved by using channel inserts. I have some cross-sections if you'd like to take a look at them I can forward the images. all the best, Helen. Dr Helen Berney, MIEEE MEBF National Microelectronics Research Centre, Prospect Row, Cork, Ireland Tel +353-21-4904010 Fax 353-21-4270271 Email hberney@nmrc.ie Webpage http://www.nmrc.ie/research/transducers-group/index.html Amanda Plimmer wrote: > Hi > > Does anyone out there have any experience of plating a metal ( I am trying > copper) into the structure of SU-8? What technique is used and what results > are obtained? Hope someone can help! > > Amanda Plimmer > Denning Group > Inorganic Chemistry Lab > University of Oxford > > ------------------------------------------------ > Amanda Plimmer > Lincoln College > Turl St > Oxford > OX1 3DR > > 07899 988238 > internal ext. 20979 > > _________________________________________________________________ > MSN Photos is the easiest way to share and print your photos: > http://photos.msn.com/support/worldwide.aspx > _______________________________________________ > mems-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.mems-exchange.org/