What region of the spectrum are you interested in? I can tell you that
the spectral features in the DUV-UV depend very much on the plasma's
properties, e.g. electron density, pressure, DC or RF (and frequency)
driving etc..

-Mike


>>> eennf@ECU-01.NOVELL.LEEDS.AC.UK 04/05/02 02:43AM >>>
Hi all,

I'm not sure if this is a bit of an obscure one (maybe I should look
for a physics discussion group!!), but does anyone have any
information (or directions to information) on the spectral output of
an argon plasma?

Thanks in advance,

Novak Farrington
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply