durusmail: mems-talk: etch al2o3
etch al2o3
2002-04-10
2002-04-10
2002-04-10
etch al2o3
David Kelly
2002-04-10
Does someone know how to etch a sputtered layer of Al2O3 without attacking the
aluminum metal layer underneath?  Note that I am not interested in simply
removing a native oxide layer.  If anyone could give some insight, it would be
greatly appreciated.

THANKS!

reply