Searching for a thin conductive material
Chunjun Wang
2002-04-10
You might want to try ACF(Anisotropic Conductive Film). Sony Chemical sells
this kind of film. But I am not sure you can make them less than 1 um thick.

Good luck!

-----Original Message-----
From: Bo He [mailto:hezhenbo@hotmail.com]
Sent: Monday, April 08, 2002 8:20 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] Searching for a thin conductive material

Hello everyone:

         I am looking for a CONDUCTIVE material which is FLEXIBLE (i.e.
polymer) and can be made very THIN (about 1um or less, possible?). Can
anyone who has experience on this give me suggestions? Any input is
highly appreciated.

Bo



------------------------------------------------------------------------

Send and receive Hotmail on your mobile device: Click Here
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply