Dear fellow MEMS Researchers, In my experiment, I use PMMA (Microchem) as sacrificial layer. The process is following, First spincoat PMMA at 800rpm for 30 sec, and prebake at 180 centi degree for 1 hours. And then deposit the other kind of material at 95 centi degree for over 30 hours. When experiment finished, I use acetone to remove the PMMA. But I find it is very difficult to remove PMMA layer completely. I have tried water bath at 70 centi degree, but there are no obviously change. Has anybody done this before? Any suggestion are highly appreciated. Cheers Peng >========================================= >Dr. P. Jin >Research Associate >School of Manufacturing and Mechanical Engineering >The University of Birmingham >Edgbaston, Birmingham B15 2TT >Tel: ++44-121-414-4256 >=========================================