The answer is yes it will damage the silicon to rie etch the nitride from the surface. You will probably already have a ghost pattern after you remove the side that was etched. If you use hot phosphoric acid in a reflux jar or system you can remove the nitride without damaging the silicon surface. Bob Henderson