Hello to everybody, is there someone who has experience in wet etching of TiW? I use a mixture of HCl and H2O2, but it seems that there are small amounts of TiW on the wafer after etching. Has someone experiences with parameters like temperature, time, other mixtures or something else? Many thanks for your help Anke