The design deadline for the 9th ARPA-supported Multi-User MEMS Processes
(MUMPs) run is scheduled for August 14, 1995.

MUMPs is available to all domestic (USA and Canada) industry, academic and
government parties. Participants may purchase a 1 cm x 1 cm die location for
$500 with approximately 15 unreleased die delivered. Layout service and die
releasing are available at an additional cost. Design rules and process
specifications are available from MCNC. Please send email to mems@mcnc.org
asking for the MUMPs design rules. Please include your snailmail address, phone
and fax numbers.

***Please note, if you already have a design rule document, be sure it is
revision 3 (10/94).***

For more information or to reserve a die location, send email to Dave Koester <
koester@mcnc.org> or call 919-248-1493.

More information on MUMPs, including the schedule for upcoming runs, is
available at the following web site:

http://www.mcnc.org/HTML/ETD/MEMS/memshome.html