Try searching google for "Laser Cut Stencils". Companies will cut stencils (usually used for squeegeeing on solder paste) out of stainless steel sheets, for reasonable prices... David Nemeth Senior Process Engineer Sophia Wireless, Inc. 14225-C Sullyfield Circle Chantilly, VA Ph: (703) 961-9573 x206 Fax:(703) 961-9576 -----Original Message----- From: mems-talk-admin@memsnet.org [mailto:mems-talk-admin@memsnet.org]On Behalf Of Stephen Bart Sent: Thursday, May 09, 2002 6:05 PM To: mems-talk@memsnet.org Subject: [mems-talk] Shadow masks I am looking for vendors who can construct a 6 in shadow mask with 1 mil (25um) or better resolution. Any suggestions? -- ******************************************************************* Stephen F. Bart, Ph.D. Technical Fellow, Core Technology Development Coventor, Inc. 625 Mount Auburn Street Cambridge, MA 02138 USA ******************************************************************* _______________________________________________ mems-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.mems-exchange.org/