Stephen, Can you provide more details as to the pattern and aspect ratios involved? Have you considered using Silicon? How about Fotofab? I've never used them, but it looks like they can do about 1/2 mil over 6": http://www.fotofab.com/Design_Considerations/Tolerances/tolerances.html Neal Stephen Bartwrote: I am looking for vendors who can construct a 6 in shadow mask with 1 mil (25um) or better resolution. Any suggestions? -- ******************************************************************* Stephen F. Bart, Ph.D. Technical Fellow, Core Technology Development Coventor, Inc. 625 Mount Auburn Street Cambridge, MA 02138 USA ******************************************************************* _______________________________________________ mems-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.mems-exchange.org/ Yahoo! Shopping - Mother's Day is May 12th!