durusmail: mems-talk: Indium Etch
Indium Etch
2002-05-31
2002-05-31
2002-05-31
2002-06-02
Indium Etch
Milan Buncick
2002-05-31
Hi all,
        Can someone please recommend an etch recipe for indium metal.
Thanks,
Milan

Dr. Milan Buncick
Director, MEMS/Photonics
The AEgis TEchnologies Group Inc.
655 Discovery Drive
Suite 301
Huntsville, AL 35806

reply