durusmail: mems-talk: Indium Etch
Indium Etch
2002-05-31
2002-05-31
2002-05-31
2002-06-02
Indium Etch
Bill Moffat
2002-05-31
First thought is lift off, let me know if I can help or you need any technical
papers.  Bill Moffat

-----Original Message-----
From: Milan Buncick [mailto:mbuncick@aegistg.com]
Sent: Friday, May 31, 2002 8:57 AM
To: Mems-Talk (E-mail)
Subject: [mems-talk] Indium Etch


Hi all,
        Can someone please recommend an etch recipe for indium metal.
Thanks,
Milan