Hi, 1) you will need to use something in the line of: BCl3 (heavy molecule) and (or CF4) to remove the 'native oxide on Al'. 2) then followed by Cl2/CHF3 to etch and provide anistropy for Al. (can't remeber the ratio)high power (2hrs?) 3) you will then need to do a 'fluorine exchange', using CF4 to remove 'Cl' to minimise corrosive HCl. 4) optional = may require a 'despeckle'. 5) once in atmosphere, you will need to quickly 'DI water (and something else) to it - a wash. I'm sure someone else can proved further detail on this subject matter. good luck. -----Original Message----- From: lib zhou [mailto:libzhou@yahoo.com] Sent: 10 June 2002 14:22 To: mems-talk@memsnet.org Subject: [mems-talk] How to plasma etch Al? Dear all; I want to plasma etching Al film, in my experiment, the Al film thickness is 300nm~500nm, using photoresist AZ3100 as etching mask, I have CHF3,SF6,O2,He2,Cl2, can you give me some advice about how to etching Al film? what's the recipe?what's the important things must be noticed in the experiments? thank you very much ahead! best regards, Lib. Sign-up for Video Highlights of 2002 FIFA World Cup _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ *************************************************************************** This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender. You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person. ***************************************************************************