Hi Masahiro Tsugai, I went through your question on mems-talk sent by you today. According to the handbook I have on "LSI process technology", the thermal expansion coefficient of TiN is 6.3x10-6 @20degC. I am sure this value is trustworthy. Tsukasa ----- Original Message ----- From: "Masahiro Tsugai"To: Sent: Wednesday, June 12, 2002 5:23 PM Subject: [mems-talk] TiN > Dear friends, > > I would like to get information regading tecnical papers > dealing with thermal expantion coefficient of TiN thin layer. > > Thanks in advance. > Masahiro > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/