Martin, Try contacting Professor John Booske at the University of Wisconsin at Madison: http://www.engr.wisc.edu/ece/faculty/booske_john.html He is affiliated with UW's Center for Plasma Aided Manufacturing: http://cpam.engr.wisc.edu/ I spoke with him last several years ago, but at that time he was researching a plasma deposition process he called Ionized Metal Vapor Deposition. Basically it involved applying a bias voltage to a metal substrate (to be coated), generating a plasma, and then sputtering a coating metal which was vaporized and attracted to the substrate. As I recall he could coat just about any metal layer onto any metal substrate with excellent conformal coating characteristics, even into very deep, high aspect ratio holes. He showed me an object with lots of intricate machining, including tapped screw holes, which had been uniformly coated with another metal using this process. I don't know if he is still involved in this project or not, but he should be a good contact on the subject. Good luck. Regards, marc -- Marc Straub Staff Engineer, Product Development Services Coventor, Inc. (Formerly Microcosm Technologies) 7 Corporate Park, Suite 260 Irvine, CA 92606 Ph: 949-756-0033 Fax: 949-756-0070 marc.straub@XXXXcoventor.com [take out the XXXX] > Message: 1 > To: mems-talk@memsnet.org > From: "Martin De_Kegelaer"> Date: Wed, 12 Jun 2002 16:50:01 +0200 > Subject: [mems-talk] reflective coating > Reply-To: mems-talk@memsnet.org > > Dear Mems specialists, > > I am searching for a way to deposit a high reflective coating inside small > holes in PC. > These holes are about 10um radius and 100um deep. > Any suggestions about the technology to use? > Could Al sputtering give a good coverage and what is the reflection% could > we expect? > > Any help is highly appreciated. > > Thanks, > > Martin De Kegelaer > > *************************************************************** > Martin De Kegelaer > Agfa-Gevaert N.V. > Research Center on Electronic Imaging > Septestraat 27, > 2640 Mortsel > Belgium > tel: +32 3444 6243 > fax: +32 3444 6450 > ***************************************************************