Hi, Hoyin, I am using a 25micron-diameter Al-Si(1%Si) wire for bonding to platinum pads. The smallest pad I have ever tried is 150micron-width x 300micron-length. Thickness of the pad is 0.2micron. I have tried Au wire too. Both wires bond well on Pt pads. Good luck, Tsukasa ----- Original Message ----- From: "Chan Ho Yin"To: Sent: Thursday, June 13, 2002 8:15 PM Subject: [mems-talk] Wire bond on Platinum bonding pad > Hi all, > > I would like to ask whether I can bond a wire on the Platinum pad by > using wire bonder. Also if it can, what is the minmium thickness and size > for the Platinum pad? Thank you very much. > > Yours, > Hoyin > > > _________________________________________________________________ > (O%N%~2y3L&h$H(O%N*:9q$l6l%s*A0H MSN Hotmail!Ghttp://www.hotmail.com > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/