durusmail: mems-talk: Tin Oxide etchant
Tin Oxide etchant
2002-06-23
2002-06-24
2002-06-25
Tin Oxide etchant
David Nemeth
2002-06-24
According to the Handbook of Metal Etchants (CRC), Tin Oxide is very
difficult to etch with a wet etch.  The only etch they suggest uses HBr
(Hydrobromic Acid), which is VERY noxious stuff.  Your best bet would
probably be a mechanical etch (RIE, Ion Milling, etc.).

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: mems-talk-admin@memsnet.org [mailto:mems-talk-admin@memsnet.org]On
Behalf Of aslam muhammad
Sent: Sunday, June 23, 2002 4:16 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Tin Oxide etchant


Hi all,
what could be etchant for tinoxide ( SnO2 ), plz

thankx

M. Aslam
Yahoo! - Official partner of 2002 FIFA World Cup
http://fifaworldcup.yahoo.com
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply