A supplier we use for of the shelf FOUP is ASSYST a local California company. They have extensive experience and numerous models all qualified in the 300 mm field. Let me know if you need any more info. Bill Moffat -----Original Message----- From: Renie M Duvall [mailto:renieduvall@earthlink.net] Sent: Wednesday, June 19, 2002 5:32 PM To: mems-talk@memsnet.org Subject: [mems-talk] Request for Supplier(s) Mems Community, I am looking for anyone who can supply FOUPS (It is a Front Opening Unified Pod) packaging for 300 mm silicon for a project. Also need to be able to locate a supplier who will provide my 300mm wafers with OCR, Data Matrix, and/or barcode marking on them. Anyone having knowledge of such please advise. --- Renie M Duvall, Kmbh--- renieduvall@earthlink.net _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/