Hi, there, use 1 M NaOH to dissolve the alumina. shimin pm72 wrote: > I was wondering if there is a solution which can dissolve both Au and alumnina > template. I need to dissolve the alumina template which is back sputtered > with gold and then release nickel nanowires .Can any one give me the details? > > fabbi. > > PHANEENDRA MEDIDA > Research Assistant > Magnetic MEMS(Dr.Gary Friedman), > Drexel University, > Philadelphia PA 19104 > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/