AZ4562 or other thick photoresist
Qingwei Mo
2002-07-03
You can try AZ9260 which can be 10-20um easily.
Qingwei

-----Original Message-----
From: mems-talk-admin@memsnet.org [mailto:mems-talk-admin@memsnet.org]On
Behalf Of hzeng
Sent: 2002?7?2? 13:12
To: mems-talk@memsnet.org
Cc: mems-talk-admin@memsnet.org; Hongjun Zeng
Subject: [mems-talk] AZ4562 or other thick photoresist


Dear Collegues,

Could you help me to reach the answer of following questions,

1. Where can I get the AZ4562 photo resist, especially in US?
2. Is there any extreme thick photoresist else which can be easily removed
by chemical liquid such as acetone?

Thanks for your attention,

Hongjun Zeng
Microfabrication Applications Laboratory (MAL)
University of Illinois at Chicago
ERF Building, 842 W. Taylor Street
Chicago, IL 60607-7022
Room 3014 ERF
Tel.: 312-413-5889, Fax: 312-996-6465
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply