durusmail: mems-talk: PDMS etching
PDMS etching
2002-07-10
2002-07-10
PDMS etching
Heiko van der Linden
2002-07-10
Hi Keyur,

I think that HF etch will work and maybe a fluoride based
dry etch too.

Heiko

*******************************
MESA+ Research Institute
      Twente University
         P.O. Box 217
     7500 AE Enschede
       The Netherlands
*******************************


-----Original Message-----
From: mems-talk-admin@memsnet.org [mailto:mems-talk-admin@memsnet.org]
On Behalf Of Keyur Shah
Sent: Wednesday, July 10, 2002 7:20 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] PDMS etching


Hello everybody,

I want to etch PDMS for my research work. Can anybody
suggest me the ways to etch it? Is it possible to etch
PDMS by using oxygen plasma? if yes, what is the etch
rate?

Thanking you all in anticipation,

Keyur Shah

=====
Keyur Shah
M.S(Chemical Engineering), Louisiana Tech University
Research Assistant, Louisiana Tech University
Apt#12, 106, South Homer Street,
Ruston, Louisiana-71270,USA.
phone no:318-513-9240
Sign up for SBC Yahoo! Dial - First Month Free http://sbc.yahoo.com
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply