I met such a problem previousely, but it has been removed when the e-beam current is promoted slowly enough. You may need to monitor the evaporation frequently in the crucible during the whole current-promoting process. Good Luck, Hongjun Zeng Message: 2 From: "Zhihai Zhang"To: Date: Thu, 11 Jul 2002 14:27:23 -0600 Subject: [mems-talk] Al evaporation Reply-To: mems-talk@memsnet.org Hello everyone, I need do Al e-beam evaporation frequently. However after several times, Al always spill out of the crucible and get the crucible cracked. I use small ramp rate, it still happened. How can I prevent it? Thnaks, Zhihai