> I am looking for MEMS foundries that are able to process 8" silicon wafers,
> medium to large volumes.
> Do you have any names/foundries that would do such things?

Carsten,

I have to second (or third...) all comments made about actual, operative
8" MEMS fabs. There are very few. The only one in Europe is right in
your back yard - Alcatel Optronics (ex Kymata) in Livingston. MEMSCAP
in Crolles is the only other one in Europe coming on-line.

With the current state of business, any mainstream wafer fab will be
happy to take on foundry business for specific processes.

Contact me off-list if you need more details.

cheers,
klaus

--

                        (TEEL)          Tokyo Electron Europe Limited
                                        PVD Process Support  (ex MRC)
Klaus Beschorner                                   Tel +49-7033-45683
Drosselweg 6                                       Fax +49-7033-45631
71120 Grafenau, Germany                       Mobile +49-174 315 7754

reply