Tom:
A thin layer of Cr will definitely help with the adhesion of Ag on Silicon.
If you must deposit directly onto a Si surface you can do an Argon presputter
clean prior to deposition and that should help with the adhesion. If you are
using an evaporator without clean capability you might want to try to plasma
clean samples and run immediately after plasma clean. Bob Henderson