durusmail: mems-talk: non-shrinking epoxy
Aluminum etch problem
Any MEMS Gyro to buy?
2002-07-23
2002-07-23
2002-07-24
non-shrinking epoxy
2002-07-25
2002-07-24
2002-07-24
non-shrinking epoxy
Yu Chang
2002-07-25
has anyone used non-shrinking epoxy which is also photo-curable or slowly
cured?
right now I'm using Devcon 2-ton non-shrinking epoxy but having the problem
to outgas the trapped air even with the use of vaccum oven.  The epoxy I'm
using becomes hardened a few minutes after the two components are mixed and
that makes the outgas very difficult.
any input will be appreciated.

Yu Chang

reply