Sorry, I should have been more specific. I have a wafer cleaning sink with megasonics etc. What I am looking for is recommended chemistries to clean the Ge wafers in. Maurice H. Norcott Senior Technician Silicon Genesis Corporation 590 Division Street Campbell, CA 95008 408-871-3948 Office 408-977-6333 Pager Mnorcott@Sigen.com