Hello, Could someone do a favor? I need information about PMMA(liquid) Polystyrene, and Polcarbonate: refraction index, absorbtion (or transparent) on 405nm wavelength, density, etc. And processing information to use them as glue. Thanks for your help Ren Yang HotJobs - Search Thousands of New Jobs http://www.hotjobs.com