Hi! The wafer temperature can climb till about 60C for thru wafer etches. Madan At 08:20 PM 5/15/2002 +0800, you wrote: >Who knows the temperature in DRIE when silicon is deep-etched, say 500microns? > >Thanks. >_______________________________________________ >mems-talk@memsnet.org mailing list: to unsubscribe or change your list >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk >Hosted by the MEMS Exchange, providers of MEMS processing services. >Visit us at http://www.mems-exchange.org/ ___________________________________________________________ K.V.Madanagopal, Ph.D. Senior Research Associate Alliance for Nanomedical Technologies 317 Stocking Hall Cornell University Ithaca NY 14850 Fax:607-255-8741 Phone:607-254-8052 ___________________________________________________________