For Plasma Activated bonding the expert to contact 1st is Dr. Shari Farrens at EVG. S.Farrens@evgroup.com EV Group Inc. 3701 University Drive, Suite 300 Phoenix, AZ 85034 Phone: 602-437-9492 ext. 146 FAX: 602-437-9435 Cell: 602-432-9406 Email: s.farrens@evgroup.com http://www: EVGroup.com -----Original Message----- From: li gang [mailto:memslg@hotmail.com] Sent: Monday, August 12, 2002 8:51 AM To: mems-talk@memsnet.org Subject: [mems-talk] plasma activated dry-bonding technology. Dear all, Could you recommand some reference on "plasma activated dry-bonding technology"? I want to know the state of art development of this technology. Besides, are there any companny offer facility to do this process (not only bonding, but also alignment included). Any information and advice will be greatly appreciated. Li Gang _________________________________________________________________ Chat with friends online, try MSN Messenger: http://messenger.msn.com _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/