You can cut a sheet of aluminum foil (say 2"x2" square), and sputter deposition for 10 minutes. Then weigh the weight gain. Assuming 99% of bulk density, you can get your rate (for gold and silver) calibrated. Yinbao Yang 704-887-3194 -----Original Message----- From: pm72 [mailto:pm72@drexel.edu] Sent: Wednesday, July 31, 2002 5:24 PM To: mems-talk@memsnet.org Subject: [mems-talk] Silver sputtering Is there are relation between the silver sputtering rate and a gold spuutering rate . please give me the details, I am trying to use this Crssington sputer coater system 108 which does not have a thickenss reader/monitor. So I have the particular readings for gold sputtering which I got from the manufacturers. I am unable to figure out the relation ship between gold and silver sputtering rates. I guess silver sputtering rate is comparitively less than gold but by HOW MUCH???? fabbi. PHANEENDRA MEDIDA Research Assistant Magnetic MEMS(Dr.Gary Friedman), Drexel University, Philadelphia PA 19104 215-895-0271 _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/