Hi, we use those mask used by the offset printing industry. They offer resolution far better than any high res laser printer, plus, one side is coated with argentum or mercury, making UV 100% unpenetrable Just ask any offset printing service provider, i'm sure they are dirt economy, even compared with high res printer and, we successfully scale down to 30um without using any lens. We actually can get 10um, but the uniformity not that good keep in contact Leow Universiti Teknologi Malaysia -------Original Message------- From: mems-talk@memsnet.org Date: Wednesday, August 21, 2002 19:44:03 To: mems-talk@memsnet.org Subject: [mems-talk] Laser printer masks Hi, i need some cheap masks; the easiest solution we found is using a laser-printer on overhead foiles. the structure size i can reach with this is so far limited to be 200microns. does anybody have experinece how to make structures smaller (without spending money on a mask) and what brands (models) of transparencies and printers might be good ? (i aim at a factor of 2 to 4 in structure size) does anybody know a place where you can buy such really cheap masks with even better resolution ? thanks already, mike _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ . [demime 0.98e removed an attachment of type image/gif]