Aqua Regia, (KI + I2), etched Nickel at approximately 100 nm/min in past
experiments.

-- Kishan Gupta
EECS Undergraduate, U.C. Berkeley

At 11:47 AM 9/9/2002 -0700, you wrote:
>Does this solution (KI(Potassium iodide)+I2(Iodine)+Water) Etch Nickel?
>