Hi.
I have used PDMS from GE Electronics (RTV 615). And I have been using
Dynasolve 210 (Dynaloy, Inc.) to dissolve the PDMS I used. It took about
less than 1 hour to dissolve 500 um thick PDMS.
Let me know if you have any questions.
Regards.

=================================
Sang Won Park
Graduate Research Assistant
Erik Jonsson School of Engineering and Computer Science
The University of Texas at Dallas
Richardson, TX 75083-0688
972-883-2893, [Fax] 972-883-6839
[E-mail] spark@utdallas.edu
[Web] http://www.utdallas.edu/~spark



----- Original Message -----
From: "flavio" 
To: 
Sent: Tuesday, September 24, 2002 12:23 AM
Subject: [mems-talk] how to remove PDMS?


>
>
>             Hello everybody,
>
>             Does anybody know how to remove (strip, clean, dissolve,
> etc.)  PDMS other way than putting it in acetone? My problem is simple,
> I've PMMA with residues of PDMS that I want to get rid of. IPA didn't
> work.
>
>
>
>             Please send an email to flavio@lsu.edu
>
>
>
>             Thanks,
>
>
>
> Flavio Aristone.
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply