durusmail: mems-talk: Polymer as mechanical structure.
Polymer as mechanical structure.
2002-10-06
Polymer as mechanical structure.
Dr. Helge Bohlmann
2002-10-07
Hello,

we produce polymer based microstructures *without tooling*. Polymers are
available with different specs.
Just let us know about the parts you need (CAD drawing or sketch) and we can
send you an offer for making them.

Best regards,

Helge Bohlmann (PhD)

microTEC
Gesellschaft für Mikrotechnologie mbH
Bismarckstr. 142 b
47057 Duisburg
Tel.: ++49 (0) 203 306 2050
Fax.: ++49 (0) 203 306 2069
Direct: ++49 (0) 203 306 2054
e-mail: bohlmann@microtec-d.com
Internet: www.microtec-d.com


----- Original Message -----
From: "li gang" 
To: 
Sent: Sunday, October 06, 2002 3:55 PM
Subject: [mems-talk] Polymer as mechanical structure.


> Dear all,
>
> Could you recommend some polymer with good mechanical charateristics?
> How to form them, by spining, PVD or CVD?
> Besides, could you tell me what's the key parameters used to evaluate
> mechanical charateristics? What's the main defects of the polymer as
> mechanical structure?
>
> Thanks in advance,
>
> Regards,
> Li Gang
>
>
>
> _________________________________________________________________
> Send and receive Hotmail on your mobile device: http://mobile.msn.com
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>




reply