Madan, I've seen green gold on very thin films ( 50A). It may be that the sticking coefficient was low due to contamination. Can you see through the green areas of the film? It may be that the film is not continuous in that area also due to contamination. Steve ----- Original Message ----- From: "Madanagopal K.V."To: Sent: Monday, October 21, 2002 11:43 AM Subject: [mems-talk] green gold > Hi, > We evaporated about 50nm gold onto glass substrates. Some greenish spots > are seen on parts of the film. Has anyone seen it before? > > Thanks > Madan > > ___________________________________________________________ > > K.V.Madanagopal, Ph.D. > Senior Research Associate > Alliance for Nanomedical Technologies > 317 Stocking Hall > Cornell University > Ithaca > NY 14850 > Fax:607-255-8741 > Phone:607-254-8052 > ___________________________________________________________ > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://www.memsnet.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ > >