Hi, I'm trying to mold a polymer device. The process is like this: polymer solution (PMMA dissolved in Acetone, for example) is injected into a fabricated mold, on which are some channels and patterns. We are expecting that the liquid polymer just flows via channel and reaches each corner of the pattern to form wanted shapes. However, the polymer inevitably flows onto to the surface of mold and eventually covers whole surface. Do you have some successful experience on such polymer molding? Best regards Yanjun(David) Tang Graduate student Institute for Micromanufacturing Louisiana Tech University 1401 Tech Farm Rd. Apt. #238, Ruston, LA 71270, USA Email: yta001@coes.latech.edu tang_yanjun@yahoo.com Tel: 1-318-255-5133