Try Super Glue, aka cyanoacrylate. It works well in TMAH and EDP. It can be dissolved it in acetone, though I've been bonding the front of wafers to chrome coated glass and then etching the chrome to release. Good luck, mike >>> skk9@cornell.edu 11/02/02 10:32AM >>> Are there materials that can used for wafer bonding that doesn't get etched/stripped in KOH bath? I've already tried Apiezon black wax, crystal bond, SU-8 (not fully crossed), but they all seems to not work quite well. I would appreciate any advice. Thanks, Kevin _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://www.memsnet.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/