I've ever developed a surface-micromachined pressure sensor specifically for oil well application. the first generation can measure pressures up to 8000 psi. the result was published in ASME: Y. Xu, F. Jiang, Y.-C. Tai, E. Donzier, W. Loomis, and A. Liberman, "A Surface Micromachined Nitride-Diaphragm High-Pressure Sensor for Oil Well Application," ASME International Mechanical Engineering Congress and Exposition, Orlando, Florida, 2000. the second generation of the sensor can measure pressure up to 14000psi with burst pressure exceeding 20000 psi. the problem is that the sensor was developed for Schlumberger. I don't know if they would like to supply this sensor. Anyway, I hope this information helps. Yong On Wed, 6 Nov 2002, Klauder, Jr., Philip R. wrote: > Friends- > > My company is looking for sensors to use at the bottom of an oil well where > the pressure can reach 6000 PSI, and the temperature can reach 160 > Centigrade. > Sensor types: > Pressure > Temperature > Viscosity > Density > Accelerometer > > Do any of you represent companies with off-the-shelf or custom sensors that > would be appropriate for this application environment? > > Phil Klauder > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://www.memsnet.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ >