Cesare,
Although we specialize in the precision bulk machining of Silicon, our facility
provides some foundry services for thin film deposition, RIE, wet etch, Metals
dep, DRIE of SIlicon, dicing and some other back end-type processes.  We also
fabricate things like thin film passives, but no active devices at this time.
You may contact me directly if your project requires some combination of this
processing suite.  I am the Fab Manager for this group.
Regards,
Neal Ricks  [nricks@shipley.com]
Shipley Co., LLC
540.552.4610x3875
 Cesare  wrote:I'd like to make contact whit companies which
fit in the "minifab"
concept. I'd like to know who are working in this way already. I was
wondering if you could contact me ....
Thanks in advance

Cesare.



_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


---------------------------------
Do you Yahoo!?
Yahoo! Web Hosting - Let the expert host your site
reply