O2 plasma is not good for reactive metals. Cr is one of the
reactive metal. Although there is a inert Au layer on top of
it, the O2 plasma can diffuse through the Au layer into the
Cr layer and then oxidise the Cr. I have the similar
experience on Au/Ti layer.