Mixing one part NH4OH with three parts H2O2 makes an effective TiW etch. Anke Stockwrote: Hi Liz, try the following 1 part HCl, 2 parts H2O2, 8 Parts H20, then heat 30 to 38 °Celsius and stir the solution. W is etched by H2O2 and Ti by HCL, the solution gets yellow. You can also take more parts of H2O2, and less water. Good luck! Anke Stock > > --__--__-- > > Message: 5 > Date: Tue, 19 Nov 2002 18:47:24 +0000 (GMT) > From: "Elizabeth.Conway" > To: mems-talk@memsnet.org > Subject: [mems-talk] query on wet etch of TiW in H202 > Reply-To: mems-talk@memsnet.org > > Hi, > what variables affect TiW etch rate in H202 in addition to temperature and low > rate. The temperature for H202 is set at 50 deg C. IS there a metallic which > catalyses TiW etch or some other variables which accelerates the etch rate, > > Regards, > Liz Conway > ______________________________________________________________________________ Ihr FreeMail-Postfach kann von jedem Telekom Festnetzanschluss erreicht werden? Mit der Voicebox - http://freemail.web.de/features/?mc=021163 _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://www.memsnet.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/ --------------------------------- Do you Yahoo!? Yahoo! Mail Plus - Powerful. Affordable. Sign up now