SU-8 once it has been hard baked should withstand both KOH and TMAH at that temperature. I am not sure whether the SU-8 will discolor however. You may consider a longer hardbake than Microchem suggests. Jennifer Pagan Senior Process Engineer WaveguideSolutions, Inc. Jpagan@WaveguideSolutions.com Phone: 704-927-0408 Fax: 704-599-3536 -----Original Message----- From: mems-talk-bounces+jpagan=waveguidesolutions.com@memsnet.org [mailto:mems-talk-bounces+jpagan=waveguidesolutions.com@memsnet.org] On Behalf Of aslam muhammad Sent: Thursday, December 12, 2002 6:34 AM To: mems-talk@memsnet.org Subject: [mems-talk] SU 8 PHOTORESIST Hi all it will be a great favour if anybody let me know whether SU 8 photoresist withstands in KOH OR TMAH ( at 90 degree celcius). thanks in anticipation M.Aslam __________________________________________________ Do you Yahoo!? Yahoo! Mail Plus - Powerful. Affordable. Sign up now. http://mailplus.yahoo.com _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/