Hello Everyone, Does anyone have information on POLYIMIDE (negative or positive, photodefinable or non, dispense or spin coat type) that can give thicknesses of sub-0.5 micron range and has a COMPRESSIVE RESIDUAL STRESS. Any help is appreciated. Regards, JSM -- Javeed Shaikh Mohammed, BIOMINDS LAB,IFM, Louisiana Tech University. Phone: (318) 257-5127 FAX: (318) 257-5104 MAIL: PO Box 10137,911 Hergot Ave. Ruston, LA 71272 ------------------------------------------------- This mail sent through IMP: http://horde.org/imp/