durusmail: mems-talk: Copper film etching solution
Copper film etching solution
N or P type SOI choice !?
2003-01-14
Copper film etching solution
yout@egr.uri.edu
2003-01-10
Hi there
I want to use FeCl3 solution to etch copper film with thickness 200nm. Does
sombody know what is the concentration of FeCl3, or any other good etching
solution for copper film. Thank you.