durusmail: mems-talk: Anyone know a good nickel etch?
Anyone know a good nickel etch?
2003-01-09
2003-01-10
2003-01-10
2003-01-10
2003-01-13
Anyone know a good nickel etch?
???
2003-01-13
How about 3:1:1(H2SO4:H2O2:H20) at 45??
I spend 15" on my nickel mask etching(6000 angstrom)
----- Original Message -----
From: "Carl Arft" 
To: 
Sent: Friday, January 10, 2003 3:41 AM
Subject: [mems-talk] Anyone know a good nickel etch?


> I'm trying to pattern nickel with photoresist.  Aqua regia seems to etch
> too quickly, and leaves some nickel un-etched.  Anyone have any other etch
> chemistries?
>
> thanks
>
> please respond to:  cmarft@ece.ucdavis.edu
>
>
>
> ********************************************
> Carl Arft
> Dept. of Electrical and Computer Engineering
> University of California, Davis
> Email: cmarft@ece.ucdavis.edu
> Phone: (530) 754-9249
> ********************************************
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply