Transene makes several copper etchants. According to their MSDS, their Copper Etchant 200 is 30% FeCl3 and 3-4% HCl, in H2O. > -----Original Message----- > From: yout@egr.uri.edu [mailto:yout@egr.uri.edu] > Sent: Friday, January 10, 2003 9:06 AM > To: mems-talk@memsnet.org > Subject: [mems-talk] Copper film etching solution > > > Hi there > I want to use FeCl3 solution to etch copper film with > thickness 200nm. Does > sombody know what is the concentration of FeCl3, or any other > good etching > solution for copper film. Thank you. > > > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ >