durusmail: mems-talk: electroless gold plating solution
electroless gold plating solution
electroless gold plating solution
Lester Lopez
2003-01-17
Kris,

Technic inc and Stapleton technologies have supplied us with electroless
nickel and gold plating solutions.  You might want to check them out at

www.technic.com

www.stapletontech.com


Lester López
Research Assistant
Microwave and Wireless Research Center
University of South Florida
4202 East Fowler Avenue, ENB 118
Tampa, Florida 33620
PH: 813-974-4851
FAX: 813-974-5250
Email: lelopez@eng.usf.edu
----- Original Message -----
From: "krishna arvindan" 
To: 
Sent: Thursday, January 16, 2003 3:13 PM
Subject: [mems-talk] electroless gold plating solution


>
> Hi,
>
> Can someone suggest me regarding vendors who can supply electroless gold
plating solution.
>
>
>
> Thanks
>
> kris
>
>
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Yahoo! Mail Plus - Powerful. Affordable. Sign up now
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply